Keyhole Formation by Laser Drilling in Laser Powder Bed Fusion of Ti6Al4V Biomedical Alloy: Mesoscopic Computational Fluid Dynamics Simulation versus Mathematical Modelling Using Empirical Validation
Data source split
- YÖKSİSYÖKSİS article record
- YÖKSİS venueNanomaterials
- Catalog match (ISSN)Nanomaterials
- OpenAlexOpenAlex enrichment (abstract, citations, topics)
Abstract
In the laser powder bed fusion (LPBF) process, the operating conditions are essential in determining laser-induced keyhole regimes based on the thermal distribution. These regimes, classified into shallow and deep keyholes, control the probability and defects formation intensity in the LPBF process. To study and control the keyhole in the LPBF process, mathematical and computational fluid dynamics (CFD) models are presented. For CFD, the volume of fluid method with the discrete element modeling technique was used, while a mathematical model was developed by including the laser beam absorption by the powder bed voids and surface. The dynamic melt pool behavior is explored in detail. Quantitative comparisons are made among experimental, CFD simulation and analytical computing results leading to a good correspondence. In LPBF, the temperature around the laser irradiation zone rises rapidly compared to the surroundings in the powder layer due to the high thermal resistance and the air between the powder particles, resulting in a slow travel of laser transverse heat waves. In LPBF, the keyhole can be classified into shallow and deep keyhole mode, controlled by the energy density. Increasing the energy density, the shallow keyhole mode transforms into the deep keyhole mode. The energy density in a deep keyhole is higher due to the multiple reflections and concentrations of secondary reflected beams within the keyhole, causing the material to vaporize quickly. Due to an elevated temperature distribution in deep keyhole mode, the probability of pores forming is much higher than in a shallow keyhole as the liquid material is close to the vaporization temperature. When the temperature increases rapidly, the material density drops quickly, thus, raising the fluid volume due to the specific heat and fusion latent heat. In return, this lowers the surface tension and affects the melt pool uniformity.
Topics
Citations
OpenAlex cited_by_count. Not a WoS or Scopus citation count; those sources have no separate column here.
28citationsOpenAlex · cited_by_count (cache / database)
7 publications in the local catalog that cite this work (OpenAlex reference match; not the full global list).
- 2021 Spatter Formation and Splashing Induced Defects in Laser-Based Powder Bed Fusion of AlSi10Mg Alloy: A Novel Hydrodynamics Modelling with Empirical TestingCitations 32 · OpenAlex
- 2022 Influence of Silicon Carbide on Direct Powder Bed Selective Laser Process (Sintering/Melting) of AluminaCitations 14 · OpenAlex
- 2021 Laser Melting Deposition Additive Manufacturing of Ti6Al4V Biomedical Alloy: Mesoscopic In-Situ Flow Field Mapping via Computational Fluid Dynamics and Analytical Modelling with Empirical TestingCitations 12 · OpenAlex
- 2022 Advances in Laser Additive Manufacturing of Cobalt–Chromium Alloy Multi-Layer Mesoscopic Analytical Modelling with Experimental Correlations: From Micro-Dendrite Grains to Bulk ObjectsCitations 10 · OpenAlex
- 2025 In-situ Dynamic laser area heating during diode point melting for thermal gradient reduction in laser powder bed fusionCitations 7 · OpenAlex
- 2025 In-situ Dynamic laser area heating during diode point melting for thermal gradient reduction in laser powder bed fusionCitations 7 · OpenAlex
- 2022 Laser additive manufacturing of Co-Cr alloy and the induced defects thereofCitations 5 · OpenAlex