Processing and Characterization of Sepiolite Clay Containing Composites for Organic Brake Pad Application

Dergi European Journal of Science and Technology
ISSN2148-2683
YÖKSİS OpenAlex Açık erişim · diamond TR Index
Yıl2020
Atıf0OpenAlex
Yüzdelik%13,7
FWCI0,01,00 = dünya ortalaması

Veri kaynağı ayrımı

  • YÖKSİSYÖKSİS makale kaydı
  • YÖKSİS dergi adıEuropean Journal of Science and Technology
  • OpenAlexOpenAlex zenginleştirmesi (özet, atıf, konular)
  • Semantic Scholaratıf sayısı (OpenAlex ile birleştirilmez)

Özet

OpenAlex Türkçe

Brake friction materials are crucial in transportation means. Organic brake pads are widely used in railway or automotive especially due to their low manufacturing cost compared to semi-metallic or ceramic pads. Owing to the complex requirements of brake lining systems, organic composite brake pads are a mixture of various components and are basically composed of binders, friction modifiers, fibers, lubricants, abrasives and various fillers. The choice of functional fillers and the optimization of the formulation is essential for improving the performances of these materials. Studies on the use of clay minerals such as kaolin or montmorillonite show that these fillers are effective. Therefore, in this study, a clay mineral, sepiolite was chosen. The composite samples prepared in this work are composed of Novolac resin as binder, cashew nut shell oil, ceramic fibers, glass fibers and other fillers. This study aims to explore the effect of sepiolite clay on the processing and on properties such as the density, the porosity or the hardness of the samples. Therefore, composite samples containing different amounts of sepiolite clay (5 wt. %, 10 wt. %, 15 wt. % and 20 wt. %) were prepared. For this purpose, the different components were mixed in a high speed mixer and pressed in a hot press at 160°C. Then, a post curing step at 180°C was applied. The density of the samples was determined and decreases from 2.22 g/cm3 to 2.10 g/cm3 with increasing sepiolite clay content. The porosity decreases from 4.47 % to 2.05% with increasing clay content until 15% and rises again to 2.81% with 20% of sepiolite content. Shore D hardness follows an inverse tendency to the density and rises from 85.3 to 90.8.

Konular

Atıflar

OpenAlex cited_by_count. WoS veya Scopus atıf sayısı değildir; o kaynaklar için ayrı kolon yoktur.

0atıfOpenAlex · cited_by_count (önbellek / veritabanı)

Yazarlar

2
  1. Bora ORAL 1
  2. ŞERİFE AKKOYUN ANKARA YILDIRIM BEYAZIT ÜNİVERSİTESİ 2