İngilizce (OpenAlex)

PURPOSE: The color of the ceramic restorations is affected by various factors such as brand, thickness of the layered the ceramic, condensation techniques, smoothness of surface, number of firings, firing temperature and thickness of dentin. The aim of this study was to evaluate the color change and surface roughness in dental porcelain with different thicknesses during repeated firings. MATERIALS AND METHODS: Disc-shaped (N=21) metal-ceramic samples (IPS Classic; Ivoclar Vivadent; Shaar, Liechtenstein) with different thickness were exposed to repeated firings. Color measurement of the samples was made using a colorimeter and profilometer was used to determine surface roughness. ANOVA and Tukey tests with repeated measurements were used for statistical analysis. RESULTS: The total thickness of the ceramics which is less than 2 mm significantly have detrimental effect on the surface properties and color of porcelains during firings (P<.05). CONCLUSION: Repeated firings have effects on the color change and surface roughness of the dental ceramics and should be avoided.

Konular

  • Dental materials and restorations
  • Dental Erosion and Treatment
  • Recycling and utilization of industrial and municipal waste in materials production

Birincil konu Dental materials and restorations

Yazarlar

  1. FEHMİ GÖNÜLDAŞ ANKARA ÜNİVERSİTESİ
  2. KEREM YILMAZ ANTALYA BİLİM ÜNİVERSİTESİ
  3. CANER ÖZTÜRK