Özet
PURPOSE: Polymer infiltrated ceramic network (PICN) materials, also called hybrid ceramics, are new materials in dental market. The manufacturer of the PICN material VITA Enamic suggests 3 different finishing procedures for this new material. In the present study, surface roughness and color differences caused from different finishing procedures of VITA Enamic were investigated. MATERIALS AND METHODS: 120 specimens were prepared in dimensions 2 × 10 × 12 mm from VITA Enamic hybrid ceramic blocks with 'high translucency' and 'translucency 2M2' shades. The specimens were divided into 8 groups. For each group, different finishing procedures suggested by the manufacturer were performed. Surface roughness values were determined by a tactile portable profilometer. Color changes were evaluated using a clinical spectrophotometer. The data were analyzed using one-way ANOVA and Tukey's post-hoc comparison. The significance level was set at α=0.05. RESULTS: The roughest surfaces were observed in Glaze Groups. Their surface roughness values were similar to that of the control group. Clinical Kit and Technical Kit groups did not show a statistically significant difference regarding surface roughness (P>.05). The largest color difference regarding ΔE00 was observed in Clinical Kit finishing groups. There were also statistically significant color changes between the groups (P<.05). However, all the groups showed clinically acceptable color change (ΔE00<2.25) except Clinical Kit Groups (ΔE00>2.25). CONCLUSION: Within the limitations of the present study, it may be suggested that finishing the VITA Enamic restorations by Technical Kit instead of Glaze and Clinical Kit gives better clinical performance in regard to surface roughness and shade matching.
Konular
Atıflar
OpenAlex cited_by_count. WoS veya Scopus atıf sayısı değildir; o kaynaklar için ayrı kolon yoktur.
75atıfOpenAlex · cited_by_count (önbellek / veritabanı)
Yerel katalogda bu makaleye atıf yapan 29 yayın (OpenAlex referans eşleşmesi; tam dünya listesi değildir).
- 2019 Effect of Different Surface Treatments on Bond Strength of Resin Cement to a CAD/CAM Restorative MaterialAtıf 118 · OpenAlex
- 2019 Effect of Different Surface Treatments on Bond Strength of Resin Cement to a CAD/CAM Restorative MaterialAtıf 118 · OpenAlex
- 2018 Optical behaviors of esthetic CAD-CAM restorations after different surface finishing and polishing procedures and UV aging: An in vitro studyAtıf 87 · OpenAlex
- 2018 Surface deterioration of monolithic CAD/CAM restorative materials after artificial abrasive toothbrushingAtıf 86 · OpenAlex
- 2018 Surface deterioration of monolithic CAD/CAM restorative materials after artificial abrasive toothbrushingAtıf 86 · OpenAlex
- 2018 Surface deterioration of monolithic CAD/CAM restorative materials after artificial abrasive toothbrushingAtıf 85 · OpenAlex
- 2017 Effects of staining liquids and finishing methods on translucency of a hybrid ceramic material having two different translucency levelsAtıf 22 · OpenAlex
- 2017 Effects of staining liquids and finishing methods on translucency of a hybrid ceramic material having two different translucency levelsAtıf 22 · OpenAlex
- 2023 Influence of Different Finishing-Polishing Procedures and Thermocycle Aging on the Surface Roughness of Nano-Ceramic Hybrid CAD/CAM MaterialAtıf 9 · OpenAlex
- 2021 Effects of Different Finishing Procedures on Surface Roughness of Hybrid CAD/CAM MaterialsAtıf 8 · OpenAlex