İçeriğe geç
akaturk Akademik ölçüm

Makale detayı · 2005

Effect of overlap length on durability of joints bonded with a pressure sensitive adhesive

Journal of Adhesion Science and Technology

YÖKSİS OpenAlex SJR Q2 JCR Q2 Atıf 14 Yüzdelik 10.4% FWCI 0.0
Yıl
2005
ISSN
0169-4243
Tür
article

Veri kaynağı ayrımı

  • YÖKSİS YÖKSİS makale kaydı
  • OpenAlex OpenAlex zenginleştirmesi (özet, atıf, konular)

Özet

İngilizce (OpenAlex)

In this study, the effect of overlap length on durability of a film type adhesive, Structural Bonding Tape (SBT) 9244, which possesses pressure-sensitive and visco-elastic properties, was investigated. Single-lap joints with 1.62 and 3.2 mm adherend thicknesses and at 12.5, 25 and 50 mm overlap lengths consisting of AA2024-T3 alloy as the adherend were exposed to two environmental conditions for exposure times of up to 90 days. The exposure environments were 100% relative humidity (RH) and 3.5% NaCl solution. At the end of exposure times, the failure surfaces were examined by Scanning Electron Microscopy (SEM) after the strength of joints was determined with the lap shear test. It was observed that with increasing overlap length, not only the failure load increased, but also the degradation rate decreased. In addition, as the metal adherends do not absorb any water and moisture from the environments, the metal adherend thickness had no effect on durability of the adhesively bonded joints.

Konular

  • Mechanical Behavior of Composites
  • Electronic Packaging and Soldering Technologies
  • Material Properties and Processing

Birincil konu Mechanical Behavior of Composites

Yazarlar

  1. Özel Adnan
  2. Temiz Şemsettin
  3. Aydin Murat Demir
  4. ADNAN ÖZEL ERZİNCAN BİNALİ YILDIRIM ÜNİVERSİTESİ
  5. MURAT DEMİR AYDIN ERZURUM TEKNİK ÜNİVERSİTESİ