İngilizce (OpenAlex)

In this study, electroless Ni-B depositions were achieved on the St-37 steel substrates at different NaBH4 concentrations and 950 oC and 1 hour. Electroless Ni-B deposited samples had a cauliflower-like surface texture that makes the electroless Ni-B deposited surface lubricating naturally and as the NaBH4 concentration increased, the grain size decreases in the microstructure. XRD spectra of the sample showed partial amorph region together with the crystalline region. Microhardness testing of the deposited samples were performed with a microhardness tester under a load of 25 g and an indentation time of 10 s. The highest hardness value was obtained in the sample prepared with 1.4 g/l NaBH4 concentration.

Konular

  • Electrodeposition and Electroless Coatings
  • Electrocatalysts for Energy Conversion
  • Corrosion Behavior and Inhibition

Birincil konu Electrodeposition and Electroless Coatings

Yazarlar

  1. YASİN YILMAZ SİVAS BİLİM VE TEKNOLOJİ ÜNİVERSİTESİ
  2. HATEM AKBULUT
  3. MEHMET UYSAL