İngilizce (OpenAlex)

The silanization process to alter the surface properties of anhydrous borax powders was investigated using an organosilane of 3-(Trimethoxysilyl) propyl methacrylate.Silanization treatments were carried out in anhydrous toluene at constant reaction temperature and silane loading.For optimizing the surface coating in the silanization processes, different processing periods (1, 6, 12, and 24 hours) were attempted.The surface-treated powders were characterized by solubility and wettability tests.

Konular

  • biodegradable polymer synthesis and properties
  • Silicone and Siloxane Chemistry
  • Surface Modification and Superhydrophobicity

Birincil konu biodegradable polymer synthesis and properties

Yazarlar

  1. SÜLEYMAN AKPINAR
  2. ZEYNİ ARSOY AFYON KOCATEPE ÜNİVERSİTESİ